I did what I usually do and “Field of Dreams’d” this thing. Went and bought a 200-gallon 3-phase 10HP compressor, filtration system, drying system, about $10K in Cerakote equipment, tidbits as well as GALLONS of H, E, C and Supergrip coatings, plus a big 7-foot PID-controlled triple oven that I could slow-roast 3 whole cows in simultaneously, as well as a nice parts bath system and Skat Blast setup.
Now we need to learn how to use it all. We’re hoping / planning to do the Certified Applicator training next month, but until then…
Do you bake your optics using 150° @ 3-hours? I assume no one bakes their Tangent Thetas at 250° for 2 hours…
Are most high-end optics/scopes, including Aimpoints and EOTechs, OK with being lightly browned at 150 for 3 hours?
Or do you just use C-series and let air cure for 5 days?
We’d like to offer coating in HIR for everything, including glass — but not sure that’s possible.
Now we need to learn how to use it all. We’re hoping / planning to do the Certified Applicator training next month, but until then…
Do you bake your optics using 150° @ 3-hours? I assume no one bakes their Tangent Thetas at 250° for 2 hours…
Are most high-end optics/scopes, including Aimpoints and EOTechs, OK with being lightly browned at 150 for 3 hours?
Or do you just use C-series and let air cure for 5 days?
We’d like to offer coating in HIR for everything, including glass — but not sure that’s possible.