Gunsmithing Painting with deep surface pitting

Stcummingsjr

Private
Full Member
Minuteman
Oct 20, 2006
13
0
Sonoma Co. California
I blasted and finished painting with Aluma-Hyde 2. Everything went well but the receiver had some deep rust marks that I hoped would fill with a thick coat- they didn’t and really detract from the paint job. I decided to strip and start again but need some advice as to what “filler” to use before my second shot of Aluma-Hyde. Thanks Steve